JE DEPA V9 Tutorial
Young's Modulus (YM) for Common Test Materials

Back Back to DEPA V9 Calibration (Step 16) Back Back to Single Item Test (Step 9)

Material

Youngs Modulus (GPa)

Youngs Modulus
lbf/in² (psi)

Rubber (small strain)

0.01-0.1

1,500-15,000

PTFE (Teflon)

0.5

75,000

Polyethylene (low density)

0.2

30,000

Polypropylene

1.5-2

217,000-290,000

Polystyrene

3-3.5

435,000-505,000

Nylon

2-4

290,000-580,000

Fiber board (medium density)

3.654

530,000

Wood (along grain)

8.963-11

1,300,000-1,600,000

High-strength Concrete (under compression)

30

4,350,000

Glass fiber reinforced plastic (70/30 by weight fibre/matrix, along grain)

40-45

5,800,000-6,500,000

Magnesium (Mg)

45

6,500,000

Aluminium (Al)

69

10,000,000

Abrasive Ceramics (vitrified/bonded)

20-90

2,900,000-13,530,000

Glass

50-90

7,251,000-13,530,000

Mother-of-Pearl (nacre, largely calcium carbonate)

70

10,000,000

Brass and Bronze

100-125

17,000,000

Titanium (Ti) and Titanium Alloys

105-120

15,000,000-17,500,000

Copper (Cu)

117

17,000,000

Carbon fiber reinforced plastic (50/50 fibre/matrix, unidirectional, along grain)

125-150

18,000,000-22,000,000

Wrought Iron

190–210

27,550,000-30,450,000

Steel

200

30,000,000

Yttrium Iron Garnet (YIG)

193-200

28,000,000-30,000,000

Beryllium (Be)

287

42,000,000

Tungsten (W)

400-410

58,000,000-59,500,000

Sapphire (Al2O3) along C-axis

435

63,000,000

Silicon Carbide (SiC)

450

65,000,000

Osmium (Os)

550

79,800,000

Tungsten Carbide (WC)

450-650

65,000,000-94,000,000

Single-Walled Carbon Nanotube

1,000+

145,000,000+

Diamond (C)

1220

150,000,000-175,000,000